Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/20/E/NS Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/30/E3 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/30/E8 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-60/40/E8 Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0301 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 IM 0240 Impact Modified Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Impact ModifierFeatures: High Density and Impact ModifiedProcessing Method: Injection MoldingInform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 0177 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 0190 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 10% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-20FG-0693 20% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-40FG-0684 40% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | |
BCC Products BC 7136 Epoxy Casting BC7136 is a gray, low toxicity, aluminum filled, epoxy casting resin. This heat resistant system may be used at room temperature without post-curing. May be cast to a thickness of ¾ inch in non-con.. |