Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.640 - 0.680 mm | 0.0252 - 0.0268 in | |
BASF Styropor® KF 462M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 18-35 kg/m3 and fire characteristics in conformity with.. |