Material Notes:
Uses: car heater casings, electrical and domestic appliance components (e.g. motor housings, dryer drums), industrial and agricultural plant components, textile bobbins.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage, Flow 0.0125 cm/cm
0.0125 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
Tensile Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
Vicat Softening Point 74.0 °C
165 °F