Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 210 cP @Temperature 30.0 °C |
210 cP @Temperature 86.0 °F |
|
Huntsman RenShape® SL 7820 Stereolithography Plastic RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appear.. |
|||
Viscosity | 210 cP @Temperature 55.0 °C |
210 cP @Temperature 131 °F |
|
BASF Pluracol® 2097 Molded Foam Polyol Description: Pluracol® 2097 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams, one-shot semi-flexible and microcellular foams. HR foams made with.. |
|||
Viscosity | 210 cP @Temperature 45.0 °C |
210 cP @Temperature 113 °F |
|
BASF Pluracol® 4156 Slabstock Foam Polyol Description: Pluracol® 4156 polyol is a 56 hydroxyl number (nominal 3000 molecular weight) polyether triol capable of producing a broad range of flexible slabstock polyurethane foams for furniture,.. |
|||
Viscosity | 210 cP @Temperature 37.8 °C |
210 cP @Temperature 100 °F |
|
BASF Pluracol® 726 Specialty Polyol Description: Pluracol® 726 polyol is a 3000 molecular weight propylene oxide adduct of glycerine. Originally designed as a slabstock foam polyol, Pluracol 726 has found wide acceptance in specialty.. |