Physical Properties Metric English Comments
Density 1.00 g/cc

@Temperature 35.0 °C
0.0361 lb/in³

@Temperature 95.0 °F
BASF Pluracol® 1135i Specialty Polyol
Description: Pluracol® 1135i polyol is a nominal 1500 molecular weight triol. Pluracol 1135i has been prepared for applications in flexible slabstock foams and polyurethane adhesive and sealants ap..
Density 1.00 g/cc

@Temperature 37.8 °C
0.0361 lb/in³

@Temperature 100 °F
BASF Pluracol® 1538 Slabstock Foam Polyol
Description: Pluracol® 1538 polyol is intended for the production of Visco-Elastic foam typically formulated with another base product such as Pluracol 593 polyol. The combination of these two immi..
Density 1.00 g/cc

@Temperature 55.0 °C
0.0361 lb/in³

@Temperature 131 °F
BASF Pluracol® 1603 Molded Foam Polyol
Description: Pluracol® 1603 polyol is a primary hydroxyl terminated polyether polyol containing an LVI inhibitor package making it ideal for molded seating foam applications. It has an actual funct..
Density 1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 220 Specialty Polyol
Description: Pluracol® 220 polyol is a high molecular weight, primary hydroxyl terminated polyol used in polyurethane elastomer and sealant formulations.Information provided by BASF
Density 1.00 g/cc

@Temperature 40.0 °C
0.0361 lb/in³

@Temperature 104 °F
BASF Pluracol® 3042 Specialty Polyol
Description: Pluracol® 3042 polyol is 41 hydroxyl number (nominal 4000 molecular weight) propoxylated polyether.Information provided by BASF
Density 1.00 g/cc

@Temperature 43.4 °C
0.0361 lb/in³

@Temperature 110 °F
BASF Pluracol® 816 Molded Foam Polyol
Description: Pluracol® 816 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol ..
Density 1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 858 Specialty Polyol
Description: Pluracol® 858 polyol is a modifying polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elast..
Density 1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
BASF Pluracol® Balance 50 Slabstock Foam Polyol
Description: Pluracol® Balance 50 polyol is a trifunctional polyether polyol based on a renewable raw material which contains mainly secondary hydroxyl groups. The polyol is capable of producing a..
Density 1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
BASF Pluracol® P2010 Specialty Polyol
Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used ..
Density 1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
BASF Pluracol® P410R Specialty Polyol
Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used ..
Density 1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
BASF Pluracol® P710R Specialty Polyol
Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used ..
Density 1.00 g/cc

@Temperature 37.8 °C
0.0361 lb/in³

@Temperature 100 °F
BASF Pluracol® TP 2540 Specialty Polyol
Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig..
Density 1.00 g/cc

@Temperature 55.0 °C
0.0361 lb/in³

@Temperature 131 °F
BASF Pluracol® 1528 FF Molded Foam Polyol
Description: Pluracol® 1528FF polyol is a graft polyol based on a high reactivity polyether triol containing approximately 45% acrylonitrile/styrene copolymer. Pluracol 1528FF is a "fine-filtered" ..
Density 1.00 g/cc

@Temperature 45.0 °C
0.0361 lb/in³

@Temperature 113 °F
BASF Pluracol® 4156 Slabstock Foam Polyol
Description: Pluracol® 4156 polyol is a 56 hydroxyl number (nominal 3000 molecular weight) polyether triol capable of producing a broad range of flexible slabstock polyurethane foams for furniture,..
Density 1.00 g/cc

@Temperature 40.0 °C
0.0361 lb/in³

@Temperature 104 °F
BASF Pluracol® 4600 Graft Slabstock Foam Polyol
Description: Pluracol® 4600 polyol is a secondary hydroxyl-terminated graft polyether triol containing approximately 44% solids of copolymerized styrene and acrylonitrile. This polyol has been form..
Density 1.00 g/cc

@Temperature 40.0 °C
0.0361 lb/in³

@Temperature 104 °F
BASF Pluracol® 4650 Graft Slabstock Foam Polyol
Description: Pluracol® 4650 polyol is a secondary hydroxyl-terminated graft polyether triol containing approximately 44% solids of copolymerized styrene and acrylonitrile. This polyol has been form..
Density 1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 726 Specialty Polyol
Description: Pluracol® 726 polyol is a 3000 molecular weight propylene oxide adduct of glycerine. Originally designed as a slabstock foam polyol, Pluracol 726 has found wide acceptance in specialty..
Density 1.00 g/cc

@Temperature 37.8 °C
0.0361 lb/in³

@Temperature 100 °F
BASF Pluracol® TP 4040 Specialty Polyol
Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig..
Density 1.00 g/cc

@Temperature 60.0 °C
0.0361 lb/in³

@Temperature 140 °F
BASF Pluracol® TP 440 Specialty Polyol
Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig..
Density 1.00 g/cc

@Temperature 48.9 °C
0.0361 lb/in³

@Temperature 120 °F
BASF Pluracol® 945 Molded Foam Polyol
Description: Pluracol® 945 polyol is a high molecular weight polyol for use in high water, low-density automotive seating foams where a high degree of foam stability is required. In combination wit..
Density 1.00 g/cc

@Temperature 40.0 °C
0.0361 lb/in³

@Temperature 104 °F
BASF Pluracol® TP 4542 Specialty Polyol
Description: Pluracol® TPE 4542 polyol is a moderately high molecular weight polyether triol that can be used in polyurethane sealant applications, flexible integral skin foam and cold-cured foam a..
Density 1.00 g/cc

@Temperature 43.3 °C
0.0361 lb/in³

@Temperature 110 °F
BASF Pluracol® 1421 Molded Foam Polyol
Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol..