Material Notes:
Description: Pluracol® 1528FF polyol is a graft polyol based on a high reactivity polyether triol containing approximately 45% acrylonitrile/styrene copolymer. Pluracol 1528FF is a "fine-filtered" version of Pluracol 1528 polyol that is designed for more stringent filters in certain graft polyol operations.Information provided by BASF
Physical Properties Metric English Comments
Density 1.00 g/cc

@Temperature 55.0 °C
0.0361 lb/in³

@Temperature 131 °F
1.01 g/cc

@Temperature 40.0 °C
0.0365 lb/in³

@Temperature 104 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 1743 cP

@Temperature 55.0 °C
1743 cP

@Temperature 131 °F
3020 cP

@Temperature 40.0 °C
3020 cP

@Temperature 104 °F
5768 cP

@Temperature 25.0 °C
5768 cP

@Temperature 77.0 °F
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Cream Opaque Liquid
Hydroxyl Number 17.0 - 21.0 mg KOH/g
STI 3007/3162