Chosun Refractories SSM-1 Special Mortar

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SSM-1 Special Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.962 MPa

@Temperature 110 °C,
Time 86400 sec
284.6 psi

@Temperature 230 °F,
Time 24.0 hour
1.962 MPa

@Temperature 500 °C,
Time 10800 sec
284.6 psi

@Temperature 932 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 <= 20 %
<= 20 %
SiO2 <= 75 %
<= 75 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C SiO2
Main Applications COKE OVEN