Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3020 cP @Temperature 40.0 °C |
3020 cP @Temperature 104 °F |
|
BASF Pluracol® 1528 FF Molded Foam Polyol Description: Pluracol® 1528FF polyol is a graft polyol based on a high reactivity polyether triol containing approximately 45% acrylonitrile/styrene copolymer. Pluracol 1528FF is a "fine-filtered" .. |