| Category | Fluid |
| Manufacturer | BASF |
| Trade Name | Lupranate® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Lupranate® MI Isocyanate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | |
| Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 10.0 - 15.0 °C | 50.0 - 59.0 °F | Freezing Point |
| Boiling Point | >= 190 °C @Pressure 0.000667 MPa |
>= 374 °F @Pressure 0.0967 psi |
|
| Flash Point | 199 °C | 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Colorless to Reddish Yellow | |
| Composition | 2,4' Isomer | 0.5 |
| Hydrolyzable Chlorine | <400 ppm | |
| NCO content | 0.335 | |
| Purity | 0.995 |