Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Softflex® SF 5560 Overmold for Nylon

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Diamond and Network Polymers
Trade Name Softflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Softflex® SF 5560 Overmold for Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 7.7 g/10 min

@Load 1.00 kg,
Temperature 235 °C
7.7 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
16.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
ASTM D2240
Tensile Strength, Yield 8.30 MPa
1200 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 650 %
650 %
chs 2.0 in/min; ASTM D638
Tear Strength 43.8 kN/m
250 pli
ASTM D624
Copyright © lookpolymers.com All Rights Reserved