Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® 227 Isocyanate Description: Lupranate® 227 Isocyanate is a liquid, modified blend product based on isomers of diphenylmethane diisocyanate (MDI). This product has good storage stability at room temperature and of.. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® 265 Isocyanate Description: Lupranate® 265 Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate 265 Isocyanate is used in the i.. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® MI Isocyanate Description: Lupranate® MI Isocyanate is pure diphenylmethane diisocyanate containing a higher amount of 2,4´ isomer than Lupranate M Isocyanate or Lupranate MS Isocyanate. Lupranate MI Isocyanate.. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® MT Isocyanate Description: Lupranate® MT Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate® MT Isocyanate is used in the .. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® MTD Isocyanate Description: Lupranate® MTD Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate® MTD Isocyanate is used in the.. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® 234 Isocyanate Description: Lupranate® 234 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high 2,4’-MDI isomer content. Lupranate® 234 Isocyanate exhibits excellent low t.. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® 241 Isocyanate Description: Lupranate® 241 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high2,4’-MDI isomer content. Lupranate® 241 Isocyanate exhibits excellent low t.. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® 78 Isocyanate Description: Lupranate® 78 Isocyanate is a polymeric MDI with a functionality of approximately 2.3. This product exhibits excellent low temperature stability. Lupranate 78 Isocyanate will remain a .. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® 81 Isocyanate Description: Lupranate® 81 Isocyanate is a carbodiimide modified pure MDI with a higher 2,4’-isomer content and a functionality of approximately 2.1. Lupranate 81 Isocyanate exhibits good low temp.. |
|||
Vapor Pressure | 4.00e-7 bar @Temperature 25.0 °C |
0.000300 torr @Temperature 77.0 °F |
|
BASF Lupranate® M Isocyanate Description: Lupranate® M Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate M Isocyanate is used in the isoc.. |