Axiall 9175 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 9175 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oil resistant tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.41 - 1.45 g/cc
1.41 - 1.45 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 86
80 - 86
delayed; ASTM D-2240
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Elongation at Yield 342 %
342 %
Oil Aging: 4 hours @ 70°C; UL 1581
342 %
342 %
Air Aging: 7 days @ 121°C; 75-mil plaques; UL 1581
360 %
360 %
ASTM D-638
100% Modulus 0.00772 GPa
1.12 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -15.0 °C
5.00 °F
ASTM D-746
Oxygen Index 28 %
28 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F