Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.2 MPa
2350 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W3201 Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon® W3201 is UL recognized for UL 94 V0 per QMFZ2, and is suitable for injection molding. This product meets UL 105°C, AWM, and Mil-W-76 80°C insulation.NOTE: Typical Properties of Molded Slab ..
Tensile Strength, Yield 16.2 - 16.7 MPa
2350 - 2420 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 16.2 - 16.7 MPa
2350 - 2420 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer
Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Teknor Apex APEX® 3201-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Teknor Apex APEX® 3301-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Teknor Apex APEX® 94-A0098A-80 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Teknor Apex Flexalloy® 3501-65-NT Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D638; ISO 527-2
Styron INSPIREâ„¢ TF1301 Thermoplastic Polyolefin
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010
Tensile Strength, Yield 16.2 MPa
2350 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SFW 5500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Footwear; General Purpose Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Tensile Strength, Yield 16.2 MPa
2350 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SGH 5500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Tensile Strength, Yield 16.2 MPa
2350 psi
20 in/min; ASTM D638
Teknor Apex Sinvicomp SMG 5500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Borealis Visico™ LE4423/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4423/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o..
Tensile Strength, Yield 16.2 MPa
2350 psi
At 20 in/min; ASTM D638
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation
Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 mas..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D638
Washington Penn Medium Impact Copolymer 40% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Borealis Visico™ LE4421/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4421/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Axiall 835WA Wire & Cable Flexible PVC
AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Axiall 9175 Wire & Cable Flexible PVC
Oil resistant tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Axiall 12860 Wire & Cable Flexible PVC
80C liquid tight conduit.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Axiall 8750 Moldings & Extrusions Flexible PVC
A clear, high quality extrusion and molding compound formulated to give good low temperature properties and good heat stability.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpora..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Axiall 8751 Moldings & Extrusions Flexible PVC
Clear, UV stabilized extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Axiall 12862 Wire & Cable Flexible PVC
Non-lead 80C liquid tight conduit compound according to UL360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D412
Borealis Visico™ LE4423/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4423/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low wire insulation and jacketing. The combina..
Tensile Strength, Yield 16.2 MPa
2350 psi
ASTM D-638
Axiall 14811 Wire & Cable Flexible PVC
Matte finish general purpose jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.