Mechanical Properties Metric English Comments
100% Modulus 0.00770 GPa
1.12 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
100% Modulus 0.00770 GPa
1.12 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
100% Modulus 0.00770 GPa
1.12 ksi
Heat aged 2 weeks at 175°C
DuPont Vamac® DP Activator OC Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00772 GPa
1.12 ksi
ASTM D-638
Axiall 9175 Wire & Cable Flexible PVC
Oil resistant tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00770 GPa
1.12 ksi
ISO 37
AlphaGary Evoprene™ 029 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
100% Modulus 0.00772 GPa
1.12 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5643Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5643Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..