Polymer Property : 100% Modulus = 0.00310 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00310 GPa
0.450 ksi
Kuraray SEPTON® S76 Soft Compound
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre..
100% Modulus 0.00310 GPa
0.450 ksi
Spartech E65450 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
100% Modulus 0.00310 GPa
0.450 ksi
Spartech M60450 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
100% Modulus 0.00310 GPa
0.450 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or..
100% Modulus 0.00310 GPa
0.450 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
100% Modulus 0.00310 GPa
0.450 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.00310 GPa
0.450 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
100% Modulus 0.00310 GPa
0.450 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s..
100% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D412
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane
Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed..
100% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00310 GPa
0.450 ksi
DIN 53504
Lubrizol ESTANE® 5735 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00310 GPa
0.450 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4640 Dense Extruded Profile
FormulationNordel® IP 4640
100% Modulus 0.00310 GPa
0.450 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4725P Dense Extrusion
FormulationNordel® IP 4725P
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D-638
Axiall 53061A Moldings & Extrusions Flexible PVC
General purpose injection molding and extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D-638
Axiall 8600 Moldings & Extrusions Flexible PVC
General purpose extrusion compound designed for use in weatherstrips, screen splines and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D412
Advanced Polymer Alloys Alcryn® 2165 TR Melt Processable Rubber
The 2100 Series grades of Alcryn® offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn®. The new 2100 grades bond to ..
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D-638
Axiall 50896 Moldings & Extrusions Flexible PVC
Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D-638
Axiall 6570 Moldings & Extrusions Flexible PVC
General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00310 GPa
0.450 ksi
ISO 37
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade)
Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible..