Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00310 GPa | 0.450 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
Kuraray SEPTON® S76 Soft Compound Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
Spartech E65450 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
Spartech M60450 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | ASTM D412 |
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane Type: Estane® AG 4350 is a polyether based aliphatic polyurethane specifically formulated to be used as an adhesive interlayer without the need for a glass surface primer. This polymer is designed.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | DIN 53504 |
Lubrizol ESTANE® 5735 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Dense Extruded Profile FormulationNordel® IP 4640 |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P Dense Extrusion FormulationNordel® IP 4725P |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | ASTM D-638 |
Axiall 53061A Moldings & Extrusions Flexible PVC General purpose injection molding and extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | ASTM D-638 |
Axiall 8600 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen splines and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2165 TR Melt Processable Rubber The 2100 Series grades of Alcryn® offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn®. The new 2100 grades bond to .. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | ASTM D-638 |
Axiall 50896 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | ASTM D-638 |
Axiall 6570 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 310ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00310 GPa | 0.450 ksi | ISO 37 |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |