Axiall 4441 Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 4441 Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
85C non-lead stabilized wire harness. SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 41 - 47
41 - 47
delayed; ASTM D-2240
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D-638
Elongation at Yield 300 %
300 %
ASTM D-638
100% Modulus 0.0141 GPa
2.05 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F