Axiall 34431 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 34431 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TW insulation. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.38 g/cc
1.34 - 1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 84 - 90
84 - 90
delayed; ASTM D-2240
Tensile Strength, Yield 16.9 MPa
2450 psi
ASTM D-638
Elongation at Yield 267.8 %
267.8 %
Air Aging: 7 days @ 113°C; 75-mil plaques; UL 1581
315 %
315 %
ASTM D-638
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -22.0 °C
-7.60 °F
ASTM D-746
Oxygen Index 25 %
25 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F