Polymer Property : 100% Modulus = 1.75 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D412
Teknor Apex UNIPRENE® 7010-50D Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.0121 GPa
1.75 ksi
Press cure 15 Minutes @ 188°C, Post Cure 16 Hours @ 250°C
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per ..
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 15880-02 Wire & Cable Flexible PVC
TW, 60C oil. 80C Class 43 insulation. Oil resistant I. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 15881 Wire & Cable Flexible PVC
80C general purpose. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 17881 Wire & Cable Flexible PVC
THW insulation compound. UL recognized component for TW, THW insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 17883 Wire & Cable Flexible PVC
UV resistant, 90C insulation compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 19881 Wire & Cable Flexible PVC
105°C rated clear compound recommended for 30 mils and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
Plasticizer conc. in vinyl film 50 phr; ASTM D638
BASF Palatinol® 11P-E (DUP) Linear Phthalate
Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing ..
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 19880 Wire & Cable Flexible PVC
105°C rated, 30 mil and larger, clear compound recommended for VW-1 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 22882 Coax & Telecom Flexible PVC
Flexible flame retardant jacket compound suitable for "patch cable" constructions over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 22883 Coax & Telecom Flexible PVC
Flexible, matte-finish, flame retardant jacket compound suitable for "patch cable" constructions over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201..
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D-638
Axiall 34431 Wire & Cable Flexible PVC
TW insulation. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0121 GPa
1.75 ksi
Dow Pellethane® 2354-55D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2354-55D is elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyureth..
100% Modulus 0.0121 GPa
1.75 ksi
ASTM D412
Dow PELLETHANE® 2355-55DE Polyurethane Elastomer, Polyester Polyadipate Based  (discontinued **)
Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting e..