Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TW363 (DAM) Nylon 46 Heat Stabilized, Impact Modified (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW363 (DAM) Nylon 46 Heat Stabilized, Impact Modified (North America).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 3.0 %
3.0 %
50% RH / 23°C; Similar to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-1/-2
Elongation at Yield >= 50 %
>= 50 %
Nominal; ISO 527-1/-2
Tensile Modulus 1.85 GPa
268 ksi
ISO 527-1/-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 7.50 J/cm²
35.7 ft-lb/in²
ISO 179/1eU
2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1
Comparative Tracking Index 475 V
475 V
IEC 60112