Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP1074KNE1 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP1074KNE1 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A nucleated, medium flow rate homopolymer resin with mold release and anti-static properties. It is suitable for general purpose injection molding.Availability: North America Features:Autoclave SterilizableEthylene Oxide SterilizableGood Creep ResistanceGood Mold ReleaseGood StiffnessSteam SterilizableUses: BottlesCapsClosuresConsumer ApplicationsPackagingProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.4 MPa
5570 psi
2.0 in/min; ASTM D638
Elongation at Yield 6.5 %
6.5 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1740 MPa
253000 psi
0.05 in/min; ASTM D790A
2010 MPa
291000 psi
0.5 in/min; ASTM D790B
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648