Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 2506 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 2506 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Tensile Modulus 2.83 GPa
410 ksi
ASTM D-638
Flexural Strength 68.9 MPa
10000 psi
ASTM D-790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D-790
Izod Impact, Notched 13.3 J/cm

@Thickness 3.17 mm
25.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Gardner Impact 0.508 J
0.375 ft-lb
per mil, Method B, C-125 Tup; ASTM D-4226
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 67.00 °C
152.6 °F
unannealed; ASTM D-648
Users viewing this material also viewed the following: