Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 45GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Volume Resistivity | 9.00e+14 ohm-cm @Temperature 100 °C |
9.00e+14 ohm-cm @Temperature 212 °F |
|
Tra-Con Tra-Bond 342-13ACC Single Component Low Viscosity Epoxy Adhesive TRA-BOND 342-13ACC single component, low viscosity epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature in 24 hours .. |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® ST120 NAT PA6-I Impact Modified, Injection Molding |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® ST145 NAT PA6-I Impact Modified, Injection Molding |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® ST220 NAT PA6-I Impact Modified, Injection Molding, Medium Viscosity |
|||
Volume Resistivity | 9.00e+14 ohm-cm @Temperature 20.0 °C |
9.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 018/13 Halogen Free PVC General purpose |
|||
Volume Resistivity | 9.00e+14 ohm-cm @Temperature 20.0 °C |
9.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 045 Halogen Free PVC General purpose; improved fire performance |
|||
Volume Resistivity | 9.00e+14 ohm-cm @Temperature 20.0 °C |
9.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 4021/TC Halogen Free PVC Improved flame retardancy |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | |
Dow Corning 3-4237 DIELECTRIC FIRM GEL KIT Two-part, translucent green, heat cure, firm, long working time, primerless chemical adhesion.Information provided by Dow Corning |
|||
Volume Resistivity | 9.00e+14 ohm-cm @Temperature 20.0 °C |
9.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 4021 Halogen Free PVC General purpose |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HF 4021/TC Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Improved flame retardancyInformation provided by Fainplast Compounds |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | 50% RH; ASTM D-257 |
Axiall 13870 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | 50% RH; ASTM D-257 |
Axiall 19911 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Volume Resistivity | 9.00e+14 ohm-cm | 9.00e+14 ohm-cm | 50% RH; ASTM D-257 |
Axiall 19912 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound recommended for various style # applications including 1007 and 1015. The compound is formulated for microbial and fungal resistance.Informatio.. |