Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Multibase Multi-Pro® 4017 C Polypropylene
Calcium Carbonate Filler, 40% by weight.Features:Stiffness, Good Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Yield 17.2 MPa
2490 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable 0800-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible)
NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength, Yield 17.2 MPa
2490 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable WR3792CL Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength, Yield 17.2 MPa
2490 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman M3019-P Polyethylene  (discontinued **)
M3019-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3019-P Has been found to exhibit good barrier properties, temperature resistance, and..
Tensile Strength, Yield 17.2 MPa
2490 psi
ASTM D638
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Global TPE-LS95A Elastomer Grade
Data provided by Global Polymers Corporation.
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Global TPO-28T Talc Filled TPO Grade
Data provided by Global Polymers Corporation.
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D412
Teknor Apex APEX® 3310-85 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Tensile Strength, Yield 17.2 MPa
2490 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SGH 5000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Techmer ES HiFill FR® PP CO FR-N
Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc.
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp..
Tensile Strength, Yield 17.2 MPa
2490 psi
ASTM D638
Eastman Tenite 485E3720023 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Tensile Strength, Yield 17.2 MPa
2490 psi
ASTM D638
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Tensile Strength, Yield 17.2 MPa
2500 psi
ISO 527-1/2
CTC X-PRO CTC PP 5002 Polypropylene Copolymer
X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
ExxonMobil LL 8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin
Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi..
Tensile Strength, Yield 17.2 MPa
2500 psi
2.0 in/min; ASTM D638
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Tensile Strength, Yield 17.2 MPa
2500 psi
2.0 in/min; ASTM D638
ExxonMobil LLP8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Axiall 02540 Plenum Flexible PVC
Non-lead stabilized Category 3 plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Axiall 1131-57D Wire & Cable Flexible PVC
Non-lead stabilized 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Axiall 17940 Wire & Cable Flexible PVC
THW insulation compound. Also suitable for 105C applications in 3/64 and larger sizes. UL recognized component for THW. Oil resistant I, VW-1 rated.Information provided by Georgia GulfGeorgia Gul..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
ExxonMobil LL 8555.67 Rotational Molding Resin  (discontinued **)
LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics ..
Tensile Strength, Yield 17.2 MPa
2490 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Axiall 01561 Plenum Flexible PVC
Non-lead stabilized CAT 5 plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 17.2 MPa
2490 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Syncure™ System S110FV-UV Polyethylene, Crosslinked (XLPE)
Syncure™ systems are two part moisture crosslinkable insulation compounds. S110FV-UV is a UL bulletinized, RoHS compliant, high strength, highly flame retardant insulation compound. Available in bl..
Tensile Strength, Yield 17.2 MPa
2500 psi
Longitudinal
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.002" thick)
Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation..
Copyright © lookpolymers.com All Rights Reserved