Material Notes:
Non-lead stabilized insulation compound recommended for 105°C applications 1/32 wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.37 g/cc
1.33 - 1.37 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
delayed; ASTM D-2240
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D-638
Elongation at Yield 231.8 %
231.8 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
315 %
315 %
ASTM D-638
100% Modulus 0.0100 GPa
1.45 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 25 %
25 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F