Teknor Apex APEX® 82-E254NL-9 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 82-E254NL-9 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 80°C Jacket; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 69
69
10 seconds; ASTM D2240
Tensile Strength at Break 22.8 MPa
3300 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use; ASTM D794
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D746
Oxygen Index 30 %
30 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque