Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Fabric Filled
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PF CC 42 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical and electrical applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.40 g/cc
1.20 - 1.40 g/cc
IEC 1212-2 7.2
Mechanical Properties Metric English Comments
Flexural Strength >= 90.0 MPa

@Diameter >=100 mm
>= 13100 psi

@Diameter >=3.94 in
Perpendicular to laminations; IEC 1212-2 4.1
Compressive Strength >= 80.0 MPa
>= 11600 psi
Axial; IEC 1212-2 4.2
Electrical Properties Metric English Comments
Insulation Resistance >= 500000 ohm

@Diameter 8.00 - 10.0 mm
>= 500000 ohm

@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Dielectric Breakdown >= 1000 V

@Temperature 90.0 °C,
Time 20.0 sec
>= 1000 V

@Temperature 194 °F,
Time 0.00556 hour
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1
>= 1000 V

@Temperature 90.0 °C,
Time 60.0 sec
>= 1000 V

@Temperature 194 °F,
Time 0.0167 hour
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1
Descriptive Properties Value Comments
Thermal Endurance 120 T.I.
IEC 1212-2 7.1
Water Absorption < 8 mg/cm²
IEC 1212-2 7.1