Austin Novel Materials Texalan® 382A Polyester-based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 382A Polyester-based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Physical Properties Metric English Comments
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 79 - 85
79 - 85
ISO 7619
Tensile Strength >= 32.0 MPa
>= 4640 psi
ISO 37
Tensile Stress >= 3.40 MPa

@Strain 100 %
>= 493 psi

@Strain 100 %
ISO 37
>= 7.50 MPa

@Strain 300 %
>= 1090 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 580 %
>= 580 %
ISO 37
Tear Strength >= 75.0 kN/m
>= 428 pli
ISO 34
K Factor (Wear Factor) <= 50
<= 50
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 40 %

@Temperature 70.0 °C
<= 40 %

@Temperature 158 °F
ISO 815