Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.40 MPa @Strain 300 % |
493 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2765 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.40 MPa @Strain 0.200 %, Temperature 80.0 °C |
493 psi @Strain 0.200 %, Temperature 176 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 3.40 MPa @Strain 26.8 %, Temperature 90.0 °C |
493 psi @Strain 26.8 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.40 MPa @Strain 74.01 %, Temperature 120 °C |
493 psi @Strain 74.01 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 3.40 MPa @Strain 5.00 %, Temperature 23.0 °C |
493 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Tensile Stress | 3.40 MPa @Strain 300 % |
493 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G65A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.40 MPa @Strain 300 % |
493 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G65A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.40 MPa @Strain 100 % |
493 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.40 MPa @Strain 100 % |
493 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.40 MPa @Strain 100 % |
493 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P55A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P55A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | >= 3.40 MPa @Strain 100 % |
>= 493 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 382A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | 3.40 MPa @Strain 100 % |
493 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P55A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P55A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |