Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.50 MPa @Strain 5.00 %, Temperature 23.0 °C |
1090 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme.. |
|||
Tensile Stress | 7.50 MPa @Strain 100 % |
1090 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EM400-BP TPC-ET 34 Shore D, Injection Molding or Extrusion Grade |
|||
Tensile Stress | 7.50 MPa @Strain 100 % |
1090 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.50 MPa @Strain 5.00 %, Temperature 23.0 °C |
1090 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® G5564 TPC-ET
(Unverified Data**) Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon .. |
|||
Tensile Stress | >= 7.50 MPa @Strain 300 % |
>= 1090 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 382A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |