Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 630-25G Nylon 6, 25% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 630-25G Nylon 6, 25% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6, 25% glass reinforced resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Ultimate 145 MPa
21000 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 6.70 GPa
972 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ASTM D648