Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass Fluon® ETFE

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE/ECTFE, Molded/Extruded
Manufacturer Asahi Glass Company
Trade Name Fluon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Fluon® ETFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and electrical properties comparable to typical fluoropolymer, such as PTFE, PFA and FEP and also is more progressive than ECTFE or PVdF with its improved mechanical strength and very easy moldability.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.74 g/cc
1.74 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Viscosity 1.00e+6 cP
1.00e+6 cP
Melt Velocity
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Hardness, Shore D 67
67
ASTM D785
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 430 %
430 %
ASTM D638
Tensile Modulus 0.800 GPa
116 ksi
ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Coefficient of Friction 0.20
0.20
Thermal Properties Metric English Comments
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 260 °C
500 °F
Maximum Service Temperature, Air 180 °C
356 °F
Continuous
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.6
2.6
ASTM D150
Dielectric Strength 120 kV/mm
3050 kV/in
ASTM D149
Dissipation Factor 0.00060

@Frequency 60 Hz
0.00060

@Frequency 60 Hz
ASTM D150
0.00080

@Frequency 1000 Hz
0.00080

@Frequency 1000 Hz
ASTM D150
0.0050

@Frequency 1e+6 Hz
0.0050

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Users viewing this material also viewed the following: