Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass Fluon® AH-3000 LM-ETFE, Conductive Type, Fluororesin

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Modified ETFE, Unreinforced
Manufacturer Asahi Glass Company
Trade Name Fluon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Fluon® AH-3000 LM-ETFE, Conductive Type, Fluororesin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive agent or surface treatment that is used at previous system. Excellent adhesiveness of the two-layer system is effected for only one step. Furthermore, the conventional properties such as anti stick, excellent moldability and chemical resistance, are same as conventional fluoro-resin.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
ASTM D792
Melt Flow 25 g/10 min
25 g/10 min
ASTM D359
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square 1000 ohm
1000 ohm
Descriptive Properties Value Comments
Permeation Rate 2.0 g-mm/m2-24hr