Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R34020W062 0.062" (1.57 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R34020W062 0.062" (1.57 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Uncured, Unsupported Silicone Rubber on a Kodacel Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Polyethylene, Interleave
127 microns
5.00 mil
Kodacel Carrier, Substrate
1420 - 1730 microns
56.0 - 68.0 mil
Overall
1420 - 1730 microns
56.0 - 68.0 mil
Side 1
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
Compound Property
Tensile Strength 8.96 MPa
1300 psi
Compound Property
Elongation at Break 600 %
600 %
Compound Property
Tear Strength 43.8 kN/m
250 pli
Compound Property
Compression Set <= 40 %
<= 40 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 177 °C
0.500 hour

@Temperature 350 °F
Recommended Cure Cycle
240 min

@Temperature 227 °C
4.00 hour

@Temperature 440 °F
Recommended Postcure Cycle
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color White
Total Product Weight (oz/yd2) 74.36 - 90.36
Users viewing this material also viewed the following: