Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1470 - 1730 microns | 58.0 - 68.0 mil | Overall |
Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci.. |
|||
Thickness | 1470 - 1730 microns | 58.0 - 68.0 mil | Overall |
Arlon R31246R063 0.063" (1.60 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 1420 - 1730 microns | 56.0 - 68.0 mil | Overall |
Arlon R34020W062 0.062" (1.57 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone Rubber on a Kodacel Carrier This data Represents typical values for the production material. The data should not be used to write, or in pla.. |
|||
Thickness | 1420 - 1730 microns | 56.0 - 68.0 mil | Side 1 |
Arlon R34020W062 0.062" (1.57 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone Rubber on a Kodacel Carrier This data Represents typical values for the production material. The data should not be used to write, or in pla.. |
|||
Thickness | 1470 - 1730 microns | 58.0 - 68.0 mil | Overall |
Arlon R34256R063 0.063" ((1.60 mm) Uncured/Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |