Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R30342R032 0.032" (0.813 mm) Cured Silicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R30342R032 0.032" (0.813 mm) Cured Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Product: Cured Silicone Rubber Liner: PolyethyleneAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Liner
813 microns
32.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
Silicone Property; ASTM D2240
Tensile Strength 9.31 MPa
1350 psi
Silicone Property; ASTM D412
Elongation at Break 800 %
800 %
Silicone Property; ASTM D412
Tear Strength 33.3 kN/m
190 pli
ASTM D624
Compression Set 20 %
20 %
Silicone Property; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Total Product Weight (oz/yd2) 37
Arlon SQA-TMS-025
Users viewing this material also viewed the following: