Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon LW201C##FR-P0 Silicone Rubber

Category Polymer , Tape , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon LW201C##FR-P0 Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Triangular cross section of self-fusing silicone tape. Interleave: 3 mil PE.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Arlon SQA-TMS-024
Thickness 508 microns
20.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
ASTM D2240
Tensile Strength, Ultimate 4.21 MPa
610 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
Adhesive Bond Strength 0.0221 MPa
3.20 psi
Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 18.3 kV/mm
465 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Char length (inches) 0.2
FAR 25.853 App.F, P.1,.Aii
Color Brown
Flame and Glow Resistance (seconds) 5
FAR 25.853 App.F, P.1,.Aii
Users viewing this material also viewed the following: