Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.3 kV/mm | 465 kV/in | ASTM D149 |
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene .. |
|||
Dielectric Strength | 18.3 kV/mm @Thickness 3.17 mm |
465 kV/in @Thickness 0.125 in |
ASTM D149 |
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Base resin for fully formulated low voltage cable i.. |
|||
Dielectric Strength | 18.3 kV/mm @Thickness 3.17 mm |
465 kV/in @Thickness 0.125 in |
ASTM D149 |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Dielectric Strength | >= 18.3 kV/mm @Temperature 121 °C, Time 10800 sec |
>= 466 kV/in @Temperature 250 °F, Time 3.00 hour |
0.0625 in. thickness; ASTM D149 |
Garlock GYLON® 3510 PTFE Gasketing, Barium Sulfate Filler PTFE with barium sulfate filler.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcellent bolt .. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | ASTM D149 |
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | Arlon SQA-TMS-020 |
Arlon 55578GA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | ASTM D149 |
Arlon LW201C##FR-P0 Silicone Rubber Triangular cross section of self-fusing silicone tape. Interleave: 3 mil PE. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | ASTM D149 |
Arlon LW301CxxFR-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 30 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M SJ-1FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M SJ-2FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Dielectric Strength | 18.3 kV/mm @Thickness 0.762 mm |
465 kV/in @Thickness 0.0300 in |
ASTM D149 |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M SJ-3FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |
|||
Dielectric Strength | 18.3 kV/mm | 465 kV/in | 7 days @ 90°C in water; ASTM D149-75 |
3M SJ-4FB Cold Shrink Foldback Splice Jacket Kits 3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice.. |