Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon AD320 Glass, PTFE and Micro-Dispersed Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon AD320 Glass, PTFE and Micro-Dispersed Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0867 lb/in³
Water Absorption 0.060 %
0.060 %
Mechanical Properties Metric English Comments
Peel Strength 2.98 kN/m
17.0 pli
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C
6.67 µin/in-°F
x direction
15.0 µm/m-°C
8.33 µin/in-°F
y direction
CTE, linear, Transverse to Flow 95.0 µm/m-°C
52.8 µin/in-°F
z direction
Thermal Conductivity 0.235 W/m-K
1.63 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1.00e+10 Hz
3.2

@Frequency 1.00e+10 Hz
3.2

@Thickness 0.508 mm
3.2

@Thickness 0.0200 in
3.2

@Thickness 2.36 mm
3.2

@Thickness 0.0930 in
Dissipation Factor 0.0038

@Frequency 1.00e+10 Hz
0.0038

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -110
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved