Arlon 56976B026 Silicone Rubber/Fiberglass Laminate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 56976B026 Silicone Rubber/Fiberglass Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
silicone property; Arlon SQA-TMS-024
Thickness 152 microns
6.00 mil
side 1; Arlon SQA-TMS-003
152 microns
6.00 mil
side 2; Arlon SQA-TMS-003
406 microns
16.0 mil
substrate; Arlon SQA-TMS-003
711 microns
28.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
silicone property; ASTM D2240
Tensile Strength, Ultimate 8.89 MPa
1290 psi
silicone property; ASTM D412
Elongation at Break 110 %
110 %
silicone property; ASTM D412
Adhesive Bond Strength 0.0221 MPa
3.20 psi
Arlon SQA-TMS-011
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 17.5 kV/mm
445 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Black