Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silicone rubber and gum on fiberglass substrateThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Side 2, Silicone Property; Arlon SQA-TMS-024
1.35 g/cc
0.0488 lb/in³
Side 1, Silicone Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Side 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Interleave
305 microns
12.0 mil
Side 2; Arlon SQA-TMS-003
406 microns
16.0 mil
Substrate; Arlon SQA-TMS-003
762 microns
30.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Side 1, Silicone Property; ASTM D2240
60
60
Side 2, Silicone Property; ASTM D2240
Tensile Strength 6.21 MPa
900 psi
Side 1, Silicone Property; ASTM D412
6.21 MPa
900 psi
Side 2, Silicone Property; ASTM D412
Elongation at Break 200 %
200 %
Side 2, Silicone Property; ASTM D412
300 %
300 %
Side 1, Silicone Property; ASTM D412
Peel Strength 1.37 kN/m
7.80 pli
Bond Strength; Arlon SQA -TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 22.0 kV/mm
560 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 177.0 °C
0.250 hour

@Temperature 350.6 °F
(under pressure) Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.0 °C
6.00 Month

@Temperature 69.8 °F
From date of manufacture
Descriptive Properties Value Comments
Color Natural
Substrate
Red
Total Product Weight (oz/yd2) 33.6
Arlon SQA-TMS-025
Users viewing this material also viewed the following: