Radici Heraform® R 3000 Acetal Copolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Radici Group Plastics
Trade Name Heraform®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraform® R 3000 Acetal Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Very easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ISO 1183
Water Absorption 0.65 %
0.65 %
ISO 62
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO 527
Elongation at Break 17 %
17 %
ISO 527
Tensile Modulus 2.90 GPa
421 ksi
ISO 527
Flexural Modulus 2.80 GPa
406 ksi
ISO 178
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ISO 75
Vicat Softening Point 151 °C

@Load 5.10 kg
304 °F

@Load 11.2 lb
ISO 306
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
Shrinkage 1.8 %

@Pressure 100 MPa,
Temperature 90.0 °C
1.8 %

@Pressure 14500 psi,
Temperature 194 °F
3 mm