Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier  (discontinued *

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier  (discontinued *.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Polyethylene Interleave
178 microns
7.00 mil
HDPE Carrier
343 - 419 microns
13.5 - 16.5 mil
Overall
343 - 419 microns
13.5 - 16.5 mil
Side 1
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 50
40 - 50
Compound Property
Tensile Strength >= 5.52 MPa
>= 800 psi
Compound Property
Elongation at Break 500 %
500 %
Compound Property
Peel Strength 1.05 kN/m
6.00 pli
Bond Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
rated per UL card E54153
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 14.2 - 17.2