| Category | Polymer , Thermoplastic , Polyether Block Amide (PEBA) |
| Manufacturer | Arkema |
| Trade Name | Pebax® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Arkema Group Pebax® MV 2080 Polyether Block Amide (PEBA).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
| Water Absorption | 48 % <br>@Temperature 23.0 °C,<br> Time 86400 sec |
48 % <br>@Temperature 73.4 °F,<br> Time 24.0 hour |
ISO 62 |
| Moisture Absorption at Equilibrium | 1.4 % <br>@Temperature 20.0 °C |
1.4 % <br>@Temperature 68.0 °F |
50% RH; ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 40 | 40 | Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868 |
| Tensile Strength at Break | 30.0 MPa | 4350 psi | Conditioned 15 days at 23°C - 50% RH; ASTM D638 |
| Elongation at Break | >= 700 % | >= 700 % | Conditioned 15 days at 23°C - 50% RH; ASTM D638 |
| Flexural Modulus | 0.0800 GPa | 11.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 160 °C | 320 °F | ISO 11357 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.502 | 1.502 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | IEC 60093 |