Material Notes:
REPOL Polypropylene H033MG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H033MG is recommended for injection molding of products where short flow paths are involved. Repol H033MG is an ideal choice for molding small industrial components, textile bobbins, caps, combs, toys etc. It is also suitable as a blending material in furniture compound. Features:Easy and consistent processabilityExcellent color and processing stabilityInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 3.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
50mm/min; ASTM D638
Elongation at Yield 11.5 %
11.5 %
50mm/min; ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648