Polymer Property : Flexural Modulus = 0.0800 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
Rotuba MSS Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
3M Dyneon™ THV 220A Fluorothermoplastic  (discontinued **)
THV 220A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate. It is soluble in ketones, esters, or ether..
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
3M Dyneon™ THV 220G Fluorothermoplastic  (discontinued **)
THV 220G is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. IT proves a balance of low temperature process..
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin
Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver..
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178
Huntsman AVALON® 95 AB Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178
LyondellBasell Hifaxâ„¢ A Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA 10 A is a thermoplastic polyolefin which has been developed for the extrusion and calendering of soft film and sheet. Thanks to its high rubber content "Hifax" CA 10 A fe..
Flexural Modulus 0.0800 GPa
11.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD801A PPE-TPE
Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements..
Flexural Modulus 0.0800 GPa
11.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Asia Pacific)
Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements..
Flexural Modulus 0.0800 GPa
11.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Europe-Africa-Middle East)
Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements..
Flexural Modulus 0.0800 GPa
11.6 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP781 PPE-TPE
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Flexural Modulus 0.0800 GPa
11.6 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Flexural Modulus 0.0800 GPa
11.6 ksi
12.5 mm/min; ISO 178
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178
DuPont Performance Polymers Hytrel® HTR8341G BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Slightly Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Flexural Modulus 0.0800 GPa
11.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MH 1657 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MH 1657 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 1657 is an inherently dissipative polymer and can be dry blended or compounded w..
Flexural Modulus 0.0800 GPa
11.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MH 2030 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MH 2030 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 2030 is an inherently dissipative polymer and can be dry blended or compounded w..
Flexural Modulus 0.0800 GPa
11.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MV 1074 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1074 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SA 01 is an inherently dissipative polymer and can be dry blended or ..
Flexural Modulus 0.0800 GPa
11.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1074 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SP 01 is an inherently dissipative polymer and can be dry blended or ..
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178; ASTM D790
Arkema Group Pebax® MV1657 Polyether Block Amide
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
3M Dyneon™ THV 221GZ Fluoroplastic Granules
3M™ Dyneon™ Fluoroplastic Granules THV 221GZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provi..
Flexural Modulus 0.0800 GPa
11.6 ksi
50% RH; ISO 178
Arkema Group Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1074 SA 01 MED is a thermoplastic elastomer made of hydrophilic flexible polyether and rigid polyamide. PEBAX® MV 1074 SA 01 MED is an inherently dissipative polyme..
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
3M Dyneon™ THV 221AZ Fluoroplastic Agglomerate
3M™ Dyneon™ Fluoroplastic Agglomerate THV 221AZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate or..
Flexural Modulus 0.0800 - 2.34 GPa
11.6 - 340 ksi
Average value: 1.16 GPa Grade Count:22
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Flexural Modulus 0.0800 GPa
11.6 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MV 2080 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 2080 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 2080 is an inherently dissipative polymer and can be dry blended or compounded w..
Flexural Modulus 0.0800 GPa
11.6 ksi
ISO 178
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..