Arkema Group OREVAC® 9307 Y EVA Terpolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Arkema
Trade Name OREVAC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 9307 Y EVA Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as free flowing natural coloured granules. Applications include skin packaging adhesive and thermo-adhesive films.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
ASTM D1505
Vinyl Acetate Content 13 - 15 %
13 - 15 %
Arkema
Melt Index of Compound 9.5 - 11.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.5 - 11.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
ASTM D2240
Tensile Strength at Break 19.0 MPa
2760 psi
ASTM D638
26.0 MPa
3770 psi
Film Property, 50 µm thickness; ASTM D882
Tensile Strength, Yield 4.80 MPa
696 psi
ASTM D638
5.60 MPa
812 psi
Film Property, 50 µm thickness; ASTM D882
Elongation at Break 600 - 900 %
600 - 900 %
ASTM D638
700 - 900 %
700 - 900 %
Film Property, 50 µm thickness; ASTM D882
Dart Drop Test 180 g
0.397 lb
ASTM D1709
Thermal Properties Metric English Comments
Melting Point 93.0 °C
199 °F
DSC
Vicat Softening Point 66.0 °C
151 °F
ASTM D1525
Ring & Ball Softening Point 145 °C
293 °F
Optical Properties Metric English Comments
Haze 3.5 %
3.5 %
50 micron film; ASTM D1003
Descriptive Properties Value Comments
MAH Mini 1600