Tensile Strength, Yield 4.80 MPa
696 psi
ASTM D412
Precision Polymer Engineering S50N Silicone Rubber
Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. To meet UK Ministry of Defence Aircraft Materials ..
Tensile Strength, Yield 4.80 MPa
696 psi
ASTM D412
Precision Polymer Engineering S60N Silicone Rubber
Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Gr..
Tensile Strength, Yield 4.80 MPa
696 psi
ASTM D412
Precision Polymer Engineering S70U Silicone Rubber
Black Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Specially formulated for anti-static, semi-conductive applications. ASTM ..
Tensile Strength, Yield 4.80 MPa
696 psi
M100
3M Dyneon™ Fluorel™ FE-5642Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle..
Tensile Strength, Yield 4.80 MPa
696 psi
M100
3M Dyneon™ Fluorel™ FC-2177 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Slower cure rate and high tear streng..
Tensile Strength, Yield 4.80 MPa
696 psi
M100
3M Dyneon™ Fluorel™ FC-2181 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Combines high elongation with excelle..
Tensile Strength, Yield 4.80 MPa
696 psi
M100
3M Dyneon™ Fluorel™ FLS-2530 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. High fluorine dipolymer with improved f..
Tensile Strength, Yield 4.80 MPa
696 psi
At 100% elongation, across flow; ASTM D412
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Tensile Strength, Yield 4.80 MPa
696 psi
50% Elongation; ASTM D412
Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical  (discontinued **)
This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r..
Tensile Strength, Yield 4.80 MPa
696 psi
ASTM D638
Arkema Group OREVAC® 9307 Y EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
Tensile Strength, Yield 4.80 MPa

@Strain 100 %
696 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1180A10 Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Copyright © lookpolymers.com All Rights Reserved