Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, .. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SABIC F00952EQ High Density Polyethylene for Blown Film Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SABIC F01552 High Density Polyethylene for Blown Film Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Dart Drop Test | 180 g | 0.397 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Dart Drop Test | 180 g | 0.397 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Dart Drop Test | 180 g | 0.397 lb | |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil LD 051.LJ Shrink Film Resin
(discontinued **) LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709A |
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil Exceed™ 1327CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327CA is a metallocene ethylene-hexene copolymers. It produces films which have high modulus whilst retaining good toughness. These properties together with excellent dr.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil Exceed™ 1327ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327ED is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327ED is fully formula.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709A |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Dart Drop Test | 180 g | 0.397 lb | 50 microns film |
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM-D1709 |
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s.. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 111 Low Density Polyethylene IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 111 is used to pr.. |
|||
Dart Drop Test | 180 g | 0.397 lb | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 113 Low Density Polyethylene IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
Arkema Group OREVAC® 9307 Y EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Dart Drop Test | 180 g | 0.397 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709A |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |
|||
Dart Drop Test | 180 g | 0.397 lb | |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Dart Drop Test | 180 g | 0.397 lb | ASTM D1709 |
Global J-4324 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |