Polymer Property : Impact Test = 26.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 35.3 J

@Temperature -40.0 °C
26.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil LD 513.48 Molding, Extrusion and Compounding Resin  (discontinued **)
LD 513.48 is a medium MI, low density polyethylene resin designed for use in compounds and masterbatches where its properties ensure improved processability and uniform dispersion of additives. The..
Impact Test 35.3 J

@Temperature 22.8 °C
26.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R20 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Impact Test 35.3 J

@Temperature 22.8 °C
26.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R26 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Impact Test 35.3 J

@Temperature 22.8 °C
26.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R84/21 Weather Resistant Sheet
Description: Weather Resistant SheetInformation provided by Spartech.
Impact Test 35.3 J
26.0 ft-lb
Torque Strength; curing at 1000°F
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..